--part1_46.276e39e7.2a126760_boundary Content-Type: text/plain; charset="US-ASCII" Content-Transfer-Encoding: 7bit In a message dated 5/14/02 2:20:51 AM Eastern Daylight Time, tesla123@pacbell.net writes: > I just read something interesting about the coatings we use. Seems all are > oil > based. The oils are cooked and blended with resins, solvents are added to > thin it, > and "metallic" dryers Bart, all, I use a water based coating. I don't know if they put any metal into it. I did some tests with the 6" x 24" toroid on the TT-42. I'll post the results later. Cheers, John --part1_46.276e39e7.2a126760_boundary Content-Type: text/html; charset="US-ASCII" Content-Transfer-Encoding: 7bit In a message dated 5/14/02 2:20:51 AM Eastern Daylight Time, tesla123@pacbell.net writes:
I just read something interesting about the coatings we use. Seems all are oil
based. The oils are cooked and blended with resins, solvents are added to thin it,
and "metallic" dryers
Bart, all,
I use a water based coating. I don't know if they put any metal
into it.
I did some tests with the 6" x 24" toroid on the TT-42. I'll post
the results later.
Cheers,
John --part1_46.276e39e7.2a126760_boundary--